Annotatsiya

Thermal treatment plays an essential role in achieving required mechanical properties of steels. Proper control of heating temperature, cooling rate, holding time, and selected cooling media determines the resulting microstructure and performance characteristics. Meanwhile, casting processes often introduce defects such as porosity, shrinkage cavities, cracks, and inclusions. These defects reduce the reliability and durability of steel components. This study examines requirements applied to steels during thermal treatment and presents effective methods for identifying and eliminating casting defects. The results show that optimized heat treatment combined with controlled casting conditions significantly enhances steel quality and operational performance.

Maqola ma’lumotlari
MualliflarRaxmatullayev Muxammadali Muxammadzokir o‘g‘li
JurnalInnores
NashriyotАндижон давлат техника университети
Nashr sanasi2025-07-31
Jild1
Son4
Betlar81-85
TilIngliz
Ilmiy sohaTexnika
Indeksga qo‘shilgan2026-08-26

Kalit so‘zlar

Heat treatment, steel thermal processing, austenitizing, quenching and tempering, cooling rate, microstructural transformation, martensite, pearlite, sorbite, casting process, casting defects

Ilmiy soha

Iqtibos keltirish

APARaxmatullayev Muxammadali Muxammadzokir o‘g‘li (2025). THERMAL TREATMENT REQUIREMENTS FOR STEELS AND CASTING DEFECT ELIMINATION. Innores, 1(4), 81-85. https://innores.uz/index.php/T/article/view/146
GOST (OAK)Raxmatullayev Muxammadali Muxammadzokir o‘g‘li THERMAL TREATMENT REQUIREMENTS FOR STEELS AND CASTING DEFECT ELIMINATION // Innores. – 2025. – T. 1, № 4. – P. 81-85.
MLARaxmatullayev Muxammadali Muxammadzokir o‘g‘li. “THERMAL TREATMENT REQUIREMENTS FOR STEELS AND CASTING DEFECT ELIMINATION.” Innores, 1(4), 81-85, 2025. https://innores.uz/index.php/T/article/view/146
ChicagoRaxmatullayev Muxammadali Muxammadzokir o‘g‘li. “THERMAL TREATMENT REQUIREMENTS FOR STEELS AND CASTING DEFECT ELIMINATION.” Innores, 1(4), 81-85 (2025). https://innores.uz/index.php/T/article/view/146
HarvardRaxmatullayev Muxammadali Muxammadzokir o‘g‘li (2025) ‘THERMAL TREATMENT REQUIREMENTS FOR STEELS AND CASTING DEFECT ELIMINATION’, Innores, 1(4), 81-85. https://innores.uz/index.php/T/article/view/146
BibTeX
@article{raxmatullayevmuxammadalimuxammadzokirogli2025,
  title = {THERMAL TREATMENT REQUIREMENTS FOR STEELS AND CASTING DEFECT ELIMINATION},
  author = {Raxmatullayev Muxammadali Muxammadzokir o‘g‘li},
  journal = {Innores},
  year = {2025},
  volume = {1},
  number = {4},
  pages = {81-85},
  url = {https://innores.uz/index.php/T/article/view/146}
}

Boshqa maqola uchun iqtibos tayyorlash

Innores jurnalidan boshqa maqolalar

Innores — barcha maqolalar · 2025-yil arxivi

Raxmatullayev Muxammadali Muxammadzokir o‘g‘li — boshqa maqolalari

Texnika sohasidagi boshqa maqolalar

Texnika sohasidagi OAK jurnallari