Features of chloridizing roasting of Almalyk mining metallurgical combinate wastes

ATAMURATOVA, Malokhat, KHAKIMBOEVA, Dildora, ShARIPOV, Khasan, KADIROVA, Zuhra, SHAKAROV, Tulkin

Kimyo va kimyo texnologiyasi · 2021-yil

Annotatsiya

With the aim to develop a comprehensive technology for processing Almalyk Mining Metallurgical Combinate (AMMC) wastes, the influence of chloride additives on the copper and zinc chloride volatilization process is considered. The relationship between presence of the calcium, potassium and sodium chlorides chlorinating additives on the copper and zinc chlorides sublimation from the AGMK wastes at roasting temperatures up to 700-1000˚C was established.

Maqola ma’lumotlari
MualliflarATAMURATOVA, Malokhat, KHAKIMBOEVA, Dildora, ShARIPOV, Khasan, KADIROVA, Zuhra, SHAKAROV, Tulkin
JurnalKimyo va kimyo texnologiyasi
Nashr sanasi2021-04-25
Betlar59-62
Tilen
DOI10.51348/kepi5028

Kimyo va kimyo texnologiyasi jurnalidan boshqa maqolalar

Kimyo va kimyo texnologiyasi — barcha maqolalar