STRESS–STRAIN CHARACTERISTICS OF ISOTACTIC POLYPROPYLENE J-170T AND BLOCK - COPOLYMER PROPYLENE WITH JM-370 ETHYLENE, DEPENDING ON TEMPERATURE AND EXTRUSION NUMBER

Q. N. Berdinazarov, N. F. Normurodov, E. O. Khakberdiev, Sh. G. Sadykov, N. R. Ashurov, A. A. Riskulov

Илм-фан ва инновацион ривожланиш · 2020-yil

Annotatsiya

Polypropylene (PP), thanks to the physicist-mechanical and temperature characteristics, are widely used in mechanical engineering and the electrical industry. In the process of thermal exposure due to degradation of PP macromolecules, a loss of elastic strength characteristics is observed. It was shown that the influence of extrusion temperatures (170-200 0С) and extrusion numbers (up to 7 cycles) lead to a strengthening of a number of mechanical properties for isotactic PP (J-170T) and practically do not affect the block copolymer of propylene with ethylene. The data obtained are of interest for the selection of polypropylene recycling conditions.

Maqola ma’lumotlari
MualliflarQ. N. Berdinazarov, N. F. Normurodov, E. O. Khakberdiev, Sh. G. Sadykov, N. R. Ashurov, A. A. Riskulov
JurnalИлм-фан ва инновацион ривожланиш
Nashr sanasi2020-09-10
Jild3
Son4
Betlar176-184
Tilen
DOI10.36522/2181-9637-2020-4-18